Which API RP recommends programs to monitor small-bore piping, flange faces, blistering and HIC/SOHIC in HF alky units?
Answer(s): B
Low creep ductility is __________ severe in high tensile strength materials and welds.
Answer(s): A
_________ is most likely found in hard weld and heat-affected zones and in high strength components.
At elevated temperature, the carbide phases in certain carbon steels are unstable and may decompose into _______. This decomposition is known as graphitization.
Hydrogen blisters may form as surface bulges on the ID, the OD on within the wall thickness of a pipe or pressure vessel. Blistering occurs from hydrogen generated by ______, not hydrogen gas from the process stream.