API API-571 Exam
Corrosion and Materials Professional (Page 3 )

Updated On: 7-Feb-2026

The sudden rapid fracture under stress (residual or applied) where the material exhibits little or no evidence of ductility or plastic deformation is called _________.

  1. 885º F Embrittlement
  2. Temper Embrittlement
  3. Stress Corrosion Cracking
  4. Brittle Fracture

Answer(s): D



What structure is 409 stainless steel?

  1. Martensitic
  2. Austenitic
  3. Duplex
  4. Ferritic

Answer(s): D



Low alloy steels contain a maximum of _______ chrome.

  1. 5%
  2. 6%
  3. 7.5%
  4. 9%

Answer(s): D



Which of the following can be affected by 885º F Embrittlement?

  1. 410 SS
  2. 430 SS
  3. 308 SS
  4. Alloy 2205
  5. A, B and D

Answer(s): E



For 5Cr-0.5Mo, what is the threshold temperature for creep?

  1. 500º F
  2. 800º F
  3. 600º F
  4. 700º F

Answer(s): B



Viewing page 3 of 92
Viewing questions 11 - 15 out of 454 questions



Post your Comments and Discuss API API-571 exam prep with other Community members:

Join the API-571 Discussion